Détails sur le produit:
|
| Type de soudure: | Soudage haute fréquence (à l'état solide) | Gamme OD du tube: | φ10-26 mm |
|---|---|---|---|
| Épaisseur de paroi: | 0,4-1,5 mm | Matière première: | Acier à faible teneur en carbone HR / CR, acier galvanisé |
| Vitesse de ligne: | jusqu'à 90 m/min | Application: | Construction légère et tube de clôture galvanisés |
| Mettre en évidence: | Galvanized Steel Tube Welding,Zinc Coated Pipe Mill,Small Diameter Galvanized Tube Line |
||
Zinc Burn-Back When Welding Galvanized Strip Galvanized coil saves a post-plating step, but welding it burns the zinc at the seam and leaves a grey, corroded line that buyers reject. Mills that overheat the weld zone also clog tooling with zinc fumes, shortening roll life and raising maintenance. Why Galvanized Strip Burns at the Weld Zinc vaporizes at a much lower temperature than steel, so an unguided or over-driven seam overheats the coating and leaves wide burn-back.
Personne à contacter: Mr. Darcy
Téléphone: 008613962217067
Télécopieur: 86-512-58371721