Détails sur le produit:
|
| Contrôle des soudures: | Guide de couture dédié + soudage par compression | Élimination des bavures: | Unité de fraisage extérieure automatique, entrée/sortie pneumatique rapide |
|---|---|---|---|
| Gamme OD du tube: | φ10-26 mm | Épaisseur de paroi: | 0,4-1,5 mm |
| Vitesse de ligne: | jusqu'à 90 m/min | ||
| Mettre en évidence: | Weld Seam Guidance Control,Squeeze Welding Steel Pipe Mill,Small Diameter Welded Tube Line |
||
Seam Drift and Incomplete Fusion in Welded Tube A weld that drifts off-center or fails to fuse completely is the fastest route to scrap and field failures. For small-diameter φ10-26mm tube, keeping the seam exactly on the squeeze-roll center is what separates a strong, round tube from a weak, oval one. Why the Weld Seam Drifts Off-Center Without a positive guide, the strip edges wander as they approach the weld point, so the squeeze rolls meet the seam off-center and fusion